Enhanced TDS
Identification & Functionality
- Product Code
- MITM10776
- RTU Product Type
- Technologies
- Product Families
Features & Benefits
- Ready-to-Use Product Features
Applications & Uses
- Application Area
Properties
- Physical Form
- Note
Polycin® 934 M-4 can be fully cured for use or test purposes at room temperature after one week. The cure can be accelerated at 60°C in 18hours, or at 80°C in 6hours.
Other
- ADR/RID/ADN Proper Shipping Name
- Chemicals, N.O.S. (POLYCIN® 934 M-4)
- ADR/RID/ADN UN Number
- Not Applicable
- Appearance (SDS)
- Clear yellow amber liquid with mild odor
- Compression Modulus
- 22.0 psi
- Dielectric Constant
- 3.3
- Electric Resistance
- 12000000000.0 Ω
- Electrical Resistivity
- 20000000000000.0 Ω-m
- Elongation at Break
- 130.0 %
- Explosive Nature (SDS)
- Not explosive
- Flammable Nature (SDS)
- Not flammable
- Flash Point
- min. 218.0 °C
- Flash Point (SDS)
- 430.0 °F
- Gel Particle Distribution
- 0.0-50.0 ppm
- Gelling Time
- 17.0-20.0 hr
- Hardness
- 55.0 HV
- Hardness
- max. 5.0 HV
- Hardness Change
- 0.0
- Hydrogen Generation
- 0.37 µl/g
- Hydrogen Generation
- 0.37 µl/g
- Insoluble in (SDS)
- Water
- Melting Point (SDS)
- -34.0 °C
- Mix Ratio
- 85.0 %(V/V)
- Other Hazards
- Not applicable.
- Oxidizing Properties (SDS)
- Not an oxidizer
- Pour Point
- -34.0 °C
- Principal
- Specific Gravity
- 0.894
- Tear Strength
- 5.0 PLI
- Tensile Modulus
- 33.0 psi
- Tensile Strength
- 25.0 psi
- Thermal Conductivity
- 0.718 BTU∙in/h∙ft²∙°F
- USA/DOT Proper Shipping Name
- Chemicals, N.O.S. (POLYCIN® 934 M-4)
- USA/DOT UN Number
- Not Applicable
- Vapor Density (SDS)
- min. 1.0 g/mL
- Viscosity
- 315.0 cPs
- Viscosity
- 300.0 cPs
- Viscosity (SDS)
- 315.0 cPs
- Volume Expansion
- 0.0 %
- Volume Resistivity
- 70000000000000.0 Ω-cm
- Water Absorption
- 0.1 %
- Water Sensitivity
- 0.0 %
- Weight Change
- 0.5 %
- Thermal Properties
Value Units Test Method / Conditions Thermal Conductivity 0.718 BTU∙in/h∙ft²∙°F BTU∙in/h∙ft²∙°F ASTM C177 - Shelf Life & Stability
Value Units Test Method / Conditions Hydrogen Generation 0.37 µl/g µl/g Gas Chromatography at 176°F, 48 h Hydrogen Generation 0.37 µl/g µl/g Mass Spectrometry (MS) at 176°F, 48 h - Electrical Properties
Value Units Test Method / Conditions Dielectric Constant 3.3 - ASTM D150 1 KHz Electric Resistance 12000000000.0 Ω Ω at 35°C, 675hr, 95% RH Electrical Resistivity 20000000000000.0 Ω-m Ω-m Volume Resistivity 70000000000000.0 Ω-cm Ω-cm ASTM D257 - Mechanical Properties
Value Units Test Method / Conditions Compression Modulus 22.0 psi psi ASTM D695 Elongation at Break 130.0 % % ASTM D412 Hardness 55.0 HV HV ASTM D1484 shore OO Hardness max. 5.0 HV HV Shore Durometer Scale at 168 hrs in boiling water Hardness Change 0.0 - Shore Durometer Scale after dry heat aging for (500 hrs, 100°C) Tear Strength 5.0 PLI PLI ASTM D624 Tensile Modulus 33.0 psi psi ASTM D638 Tensile Strength 25.0 psi psi ASTM D412 Water Sensitivity 0.0 % % Telcordia TR-NWT-000354 Expansion - Physical Properties
Value Units Test Method / Conditions Flash Point min. 218.0 °C °C ASTM D3828 Gel Particle Distribution 0.0-50.0 ppm ppm Internal Method on 150 micron Gelling Time 17.0-20.0 hr hr Internal Method at 25°C, 100g Pour Point -34.0 °C °C Specific Gravity 0.894 - ASTM D1875 Viscosity 315.0 cPs cPs ASTM D2393 At 25°C Viscosity 300.0 cPs cPs ASTM D2393 at 25°C, mixed Volume Expansion 0.0 % % Telcordia TR-NWT-000354 Water Absorption 0.1 % % at 24°F, 168 hrs in boiling water Weight Change 0.5 % % at 168 hrs in boiling water - Application Information
Value Units Test Method / Conditions Mix Ratio 85.0 %(V/V) %(V/V) - SDS Physical and Chemical Properties
Value Units Test Method / Conditions Flash Point (SDS) 430.0 °F °F Pensky-Martens Closed Cup (PMCC) Melting Point (SDS) -34.0 °C °C Vapor Density (SDS) min. 1.0 g/mL g/mL air = 1, heavier than air Viscosity (SDS) 315.0 cPs cPs at 25°C