Enhanced TDS
Identification & Functionality
- Blend
- No
- Chemical Family
- Plastics & Elastomers Functions
- Product Code
- MITM13716
- Single Ingredient
- Yes
- Technologies
- Product Families
Features & Benefits
- Materials Features
- Key Features
XIRAN® IZ1018M can be processed in all types of regular polymer processing equipment. For good dispersion in styrenic polymer like ABS, twin screw extruders with a mild screw configuration and vacuum degassing facility are recommended. To avoid product degradation, temperatures above 280°C and high shear stresses should be avoided.
Applications & Uses
- Compatible Polymers & Resins
- Product Uses
XIRAN® IZ1018M can be used with dosage levels up to 40%. The addition of XIRAN® IZ1018M can be added for enhancing temperature and dimensional stability, surface adhesion properties and melt viscosity in a number of polymer systems, specifically in ABS.
- Product Applications
XIRAN® IZ1018M is specifically designed as an additive to increase the thermal properties of several engineering plastics especially in styrenics like ABS.
Properties
- Physical Form
Regulatory & Compliance
- Certifications & Compliance
- Chemical Inventories
- Contains any chemicals listed on Prop 65 (including impurities, residues, catalysts, monomers, and by-products and excluding heavy metals)?
Packaging & Availability
- Packaging Type
Principal Information
- Group Principal Number
- S002899
- Principal
Storage & Handling
- Storage Conditions
Store at well ventilated and dry places, protected from heat and direct sunlight. Avoid excessive moisture. The granules ensure easy, dust free handling and can be added to the compounding extruder through regular feeder systems.
Other
- Appearance
- Yellow granules
- Item Number
- Odor (SDS)
- Characteristic weak
- Other Hazards
- Of no significance
- USA/DOT UN Number
- Not Applicable
- Thermal Properties
Value Units Test Method / Conditions Thermal Stability 390.0 °C Thermo-Gravimetric Analysis - Physical Properties
Value Units Test Method / Conditions Bulk Density 0.6 g/cm³ Internal Method Drying Time 2.0-3.0 hr Glass Transition Temperature (Tg) 175.0 °C ISO 3146 Melt Flow Index 50.0 g/10min ISO 1133 at 265°C, 10 kg - Material Composition
Value Units Test Method / Conditions Maleic Anhydride Content 10.0 % Internal Method - Application Information
Value Units Test Method / Conditions Application Temperature 280.0 °C Compounding Temperature 230.0-250.0 °C Dosage (Use Level) max. 40.0 % - SDS Physical and Chemical Properties
Value Units Test Method / Conditions Density (SDS) 1.1-1.2 g/cm³